Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 400 °C | 752 °F | |
Ferro EG 2739 Thick Film Glass Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, .. |
|||
Transformation Temperature | 400 °C | 752 °F | |
Ferro EG 4010 Display Device Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas.. |