Transformation Temperature 400 °C
752 °F
Ferro EG 2739 Thick Film Glass
Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, ..
Transformation Temperature 400 °C
752 °F
Ferro EG 4010 Display Device
Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas..