Thermal Properties Metric English Comments
Transformation Temperature 76.0 - 81.0 °C
169 - 178 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 820 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 76.0 - 81.0 °C
169 - 178 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 820 SL 40 Unexpanded microspheres in aqueous dispersion
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 71.0 - 81.0 °C
160 - 178 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 820 SL 80 Unexpanded microspheres in aqueous dispersion
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 76.0 - 81.0 °C
169 - 178 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 820 SLU 40 Unexpanded microspheres in aqueous dispersion
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 76.0 - 81.0 °C
169 - 178 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 820 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..