Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Akzo Nobel Expancel® 820 DU 40 Dry unexpanded microspheres

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Akzo Nobel, Expancel
Trade Name Expancel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Expancel® 820 DU 40 Dry unexpanded microspheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the thermoplastic shell softens and the gas increases its pressure, resulting in an expansion of the spheres.Applications: Anti-slip coatings; Printing ink; Car underbody coatings; Industrial non-woven textiles;
Physical Properties Metric English Comments
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Particle Size 10 - 16 µm
10 - 16 µm
D(0.5)
Thermal Properties Metric English Comments
Transformation Temperature 76.0 - 81.0 °C
169 - 178 °F
Expansion Starting Temperature
115 - 125 °C
239 - 257 °F
Temp at Max Expansion
Descriptive Properties Value Comments
Solvent Resistance 1
Scale of 1 to 5