Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | <= -76.0 °C | <= -105 °F | Freezing Point |
LG Chemical 2-EH 2-Ethyl Hexanol Applications: Plasticizers, stabilizers, solvents, acrylatesCAS: 104-76-7Information provided by LG Chemical |
|||
Melting Point | -76.0 °C | -105 °F | |
Dow Corning Z-1211 METHYLTRICHLOROSILANE Information provided by Dow Corning |