Thermal Properties Metric English Comments
Melting Point -61.0 °C
-77.8 °F
BASF Dimethylformamide
Formula: C4H11NCAS: 68-12-2Description: Dimethylformamide is a colorless to yellow liquid with a faint, specific amine-like odor. It is miscible with water.Synonyms: DMF, N,N-DimethylformamideAppli..
Melting Point -61.0 °C
-77.8 °F
Freezing Point
BASF Isobutyl Acrylate
Formula: C7H12O2CAS: 106-63-8Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Isobutyl acrylate forms homopolymers and copolymers. Copol..
Melting Point -61.0 °C
-77.8 °F
BASF Methyl Chloroformate
Formula: C2H3ClO2CAS: 79-22-1Description: Methyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: Chloroformic acid methyl este..