Polymer Property : Melting Point = 1029 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 960 - 1029 °C
1760 - 1885 °F
Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy
Characteristics:Because of the wide melting range, this filler metal has good gap filling characteristics at the lower end of the brazing range and is relatively free-flowing near the upper end. We..