Thermal Properties Metric English Comments
Melting Point 961 °C
1760 °F
After Sintering
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package..
Melting Point 960 - 1030 °C
1760 - 1890 °F
Johnson Matthey D Bronze High Temperature Alloy for Tungsten Carbide Brazing
D Bronze is primarily used for the production of rock drills. Or where simultaneous heat treatment of the steel shank is required. Information provided by Johnson Matthey.
Melting Point 960 - 971 °C
1760 - 1780 °F
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi..
Melting Point 960 - 1029 °C
1760 - 1885 °F
Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy
Characteristics:Because of the wide melting range, this filler metal has good gap filling characteristics at the lower end of the brazing range and is relatively free-flowing near the upper end. We..
Melting Point 960 - 990 °C
1760 - 1810 °F
Wieland 1703 Wilaform Gold
Yield alloy particularly suitable for coin and medal production.Applications: casting, chains, coin/shape, laminar decoration, tubingDental
Melting Point 961 °C
1760 °F
Wieland 3005 Wilaform Silver
Fine silver. Particularly suitable for minting or technical purposes.Applications: chains, coin/shape, laminar decoration, pipesDental
Melting Point 960 °C
1760 °F
Goodfellow Manganin® Copper Resistance Alloy
Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.In..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TDX Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TH1 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TH3 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 960 °C
1760 °F
CLAL-MSX DECLAFOR® 1015 TF Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Melting Point 961 °C
1760 °F
Indium Corp. Indalloy 207 Pure Silver