Melting Point 476 - 635 °C
889 - 1180 °F
Kaiser 7068 T6, T651 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
Melting Point 476 - 635 °C
889 - 1180 °F
Kaiser 7068 T6, T6511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
Melting Point 476 - 635 °C
889 - 1180 °F
Kaiser 7068 T76, T76511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
Melting Point 625 - 635 °C
1160 - 1180 °F
Johnson Matthey Mattibraze 50 Cadmium Containing Silver Brazing Alloy
Very free flowing low melting alloys which are used when there is a need to keep the brazing temperature to a minimum.Safety Precautions with Cadmium Containing Alloys: Today the potential danger fr..
Melting Point 540 - 640 °C
1000 - 1180 °F
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..
Melting Point 625 - 635 °C
1160 - 1180 °F
Indium Corp. Indalloy 216 Silver Solder Alloy
Information Provided by Indium Corporation