Indium Corp. Indalloy 216 Silver Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 216 Silver Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.19 g/cc
0.332 lb/in³
Thermal Properties Metric English Comments
Melting Point 625 - 635 °C
1160 - 1180 °F
Solidus 625 °C
1160 °F
Liquidus 635 °C
1180 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 18 %
18 %
Copper, Cu 15 %
15 %
Silver, Ag 50 %
50 %
Zinc, Zn 16.5 %
16.5 %