Thermal Properties Metric English Comments
Melting Point 51.0 - 61.0 °C
124 - 142 °F
Fine Organics FINALUX G 322 Lubricant Additive
Applications: All round lubricant for rigid PVC profiles/extrusion and injection molding, lubricant for Polycarbonate.Information provided by Fine Organics
Melting Point 51.0 °C
124 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3182 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
28 wt% Vinyl Acetate.Elvax® 3182-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..
Melting Point 51.0 °C
124 °F
Freezing Point via DSC/ASTM D3418
DuPont Bynel® 1123 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Melting Point 51.0 °C
124 °F
Freezing Point via DSC/ASTM D3418
DuPont Bynel® 1124 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Melting Point 51.0 - 89.0 °C
124 - 192 °F
ASTM D3418(DSC)
DuPont Surlyn® 9945 Thermoplastic Ionomer Resin
Surlyn® 9945 provides high flow properties and consistent, easy processing behavior in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the i..
Melting Point 51.0 °C
124 °F
Freezing Point; ASTM D3418
DuPont™ Fusabond® C250 Polymer Modifier
DuPont™ Fusabond® C250 is a modified ethylene vinyl acetate copolymer. Used as an adhesion promoter and coupling agent.
Melting Point 51.0 °C
124 °F
BASF Octamethylenediamine
Formula: C8H20N20CAS: 373-44-4Description: Octamethylenediamine is a colorless solidified mass with an amine-like odor. It is miscible with water.Synonyms: 1,8-DiamineoctaneApplications: It is used..
Melting Point 51.0 °C
124 °F
Freezing Point; ASTM D3417, ISO 3146
DuPont™ Surlyn® 1707 Sodium Ionomer
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Melting Point 51.0 - 101 °C
124 - 214 °F
Average value: 90.3 °C Grade Count:27
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..