Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 51.0 - 61.0 °C | 124 - 142 °F | |
Fine Organics FINALUX G 322 Lubricant Additive Applications: All round lubricant for rigid PVC profiles/extrusion and injection molding, lubricant for Polycarbonate.Information provided by Fine Organics |
|||
Melting Point | 54.0 - 61.0 °C | 129 - 142 °F | |
Struktol V-SSE Processing Additive Fatty acid esterTypical Applications: STRUKTOL® V-SSE has both internal and external lubricant characteristics. It is used in calendering, extrusion and injection molding applications. It also ha.. |