Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1353 - 1393 °C | 2467 - 2539 °F | |
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |