Thermal Properties Metric English Comments
Melting Point 1353 - 1393 °C
2467 - 2539 °F
Special Metals INCOLOY® alloy 864
INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma..