Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 740.6 - 788 °C | 1365 - 1450 °F | |
Lucas-Milhaupt BRAZE 750 (Hard) Silver Based Cadmium Free Filler Metal Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel.. |