Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 570 - 789 °C | 1060 - 1450 °F | |
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Melting Point | 645 - 785 °C | 1190 - 1450 °F | |
Johnson Matthey Matti-phos 2 Alloy for Fluxless Brazing of Copper This alloy is less expensive than other Matti-phos alloys. It has good flow and ductility, and has the same uses as Copper-flo.Optimum Joint Gap 0.05 - 0.2 mm.AWS A5.8-92 BCuP-6BS EN 1044 1999 CP10.. |
|||
Melting Point | 775 - 785 °C | 1430 - 1450 °F | |
Indium Corp. Indalloy 220 Silver Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 740.6 - 788 °C | 1365 - 1450 °F | |
Lucas-Milhaupt BRAZE 750 (Hard) Silver Based Cadmium Free Filler Metal Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel.. |
|||
Melting Point | 643 - 788 °C | 1190 - 1450 °F | |
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |