Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1220 - 1390 °C | 2230 - 2530 °F | |
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm.. |
|||
Melting Point | 1315 - 1390 °C | 2399 - 2530 °F | |
Goodfellow T2-Thermocouple Alloy The negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use.Information provided.. |
|||
Melting Point | 1340 - 1390 °C | 2440 - 2530 °F | |
Goodfellow Evanohm® Precision Resistance Nickel Alloy Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow. |
|||
Melting Point | 1340 - 1390 °C | 2450 - 2540 °F | |
Carlson 330 Austenitic Alloy General DescriptionCarlson Alloy 330 is a nickel-iron-chromium-silicon austenitic alloy. It combines high strength with excellent resistance to carburization and oxidation at temperatures to 2200°.. |