Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Goodfellow Evanohm® Precision Resistance Nickel Alloy

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer Goodfellow
Trade Name Evanohm®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Evanohm® Precision Resistance Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow.
Physical Properties Metric English Comments
Density 8.10 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 1210 MPa
175000 psi
Elongation at Break <= 33 %
<= 33 %
Tensile Modulus 221 GPa
32100 ksi
Izod Impact, Unnotched 0.420 - 1.00 J/cm
0.787 - 1.87 ft-lb/in
Notch Status Unknown
Thermal Properties Metric English Comments
CTE, linear 11.7 µm/m-°C

@Temperature 20.0 - 100 °C
6.50 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 14.6 W/m-K
101 BTU-in/hr-ft²-°F
Melting Point 1340 - 1390 °C
2440 - 2530 °F
Solidus 1340 °C
2440 °F
Liquidus 1390 °C
2530 °F
Maximum Service Temperature, Air 300 °C
572 °F
Component Elements Properties Metric English Comments
Aluminum, Al 2.5 %
2.5 %
Chromium, Cr 20 %
20 %
Copper, Cu 2.5 %
2.5 %
Nickel, Ni 75 %
75 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000134 ohm-cm
0.000134 ohm-cm
Temperature Coefficient of 0.00001/K
Users viewing this material also viewed the following: