Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Melting Point | 1430 °C | 2606 °F | |
Hoskins Manufacturing Chromel® Thermocouple Wire Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usageChromel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsu.. |
|||
Melting Point | 1430 °C | 2610 °F | |
Special Metals NILO® Alloy 36 Low-Expansion Alloy Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic.. |
|||
Melting Point | 1430 °C | 2610 °F | |
Goodfellow Copper 70/Iron 30 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1430 °C | 2610 °F | |
Goodfellow Nickel 80/Molybdenum 20 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1430 - 3410 °C | 2610 - 6170 °F | |
Astaras Anviloy® Weld Rod Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.Applications:R.. |
|||
Melting Point | 1430 - 1510 °C | 2600 - 2750 °F | |
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |
|||
Melting Point | 1430 - 1510 °C | 2600 - 2750 °F | |
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
Melting Point | 1430 - 1480 °C | 2600 - 2700 °F | |
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Melting Point | 1430 - 1480 °C | 2600 - 2700 °F | |
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Melting Point | 1430 °C | 2600 °F | |
California Fine Wire Alloy 52 Nickel Iron Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1430 °C | 2610 °F | |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1430 °C | 2610 °F | |
California Fine Wire Nickel 271 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1430 °C | 2610 °F | |
California Fine Wire Nickel 272 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1430 °C | 2610 °F | |
Alloy Wire International RW 122 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
Melting Point | 1430 - 1510 °C | 2606 - 2750 °F | |
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
Melting Point | 1430 - 3410 °C | 2610 - 6170 °F | |
Astaras Anviloy® Weld Rod Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.Applications:R.. |
|||
Melting Point | 1430 °C | 2600 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |