Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1430 °C | 2610 °F | |
Special Metals NILO® Alloy 36 Low-Expansion Alloy Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic.. |
|||
Melting Point | 1430 °C | 2610 °F | |
Goodfellow Copper 70/Iron 30 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1430 °C | 2610 °F | |
Goodfellow Nickel 80/Molybdenum 20 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1430 - 3410 °C | 2610 - 6170 °F | |
Astaras Anviloy® Weld Rod Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.Applications:R.. |
|||
Melting Point | 1430 °C | 2610 °F | |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1430 °C | 2610 °F | |
California Fine Wire Nickel 271 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1430 °C | 2610 °F | |
California Fine Wire Nickel 272 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1430 °C | 2610 °F | |
Alloy Wire International RW 122 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
Melting Point | 1430 - 3410 °C | 2610 - 6170 °F | |
Astaras Anviloy® Weld Rod Anviloy® is a tungsten-based TIG filler metal used for enhancing and repairing dies and inserts. These weld rods work equally as well on both tool steel and tungsten based materials.Applications:R.. |