Polymer Property : Melting Point = 144 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 62.0 - 107 °C
144 - 225 °F
Average value: 83.7 °C Grade Count:22
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
Melting Point 62.0 °C
144 °F
Exxon Method
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Melting Point 62.0 - 65.0 °C
144 - 149 °F
M Chemical GUARD DOGâ„¢ UV9 Light Stabilizer, Benzophenone Derivative
GUARD DOGâ„¢ UV9 light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout ..
Melting Point 62.0 °C
144 °F
Eutectic
Indium Corp. Indalloy 18 Indium Solder Alloy
Information Provided by Indium Corporation
Melting Point 62.0 °C
144 °F
Solvay Chemicals Ethyl 3-(difluoromethyl)-1-methyl-1H-pyrazole-4-carboxylate
CAS-No.: 141573-95-7 / EC-No.: 619-510-5 Uses: Chemical intermediateInformation provided by Solvay
Melting Point 62.0 °C
144 °F
ASTM D3418 - ISO 3146
DuPont Elvaloy® HP661 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Melting Point 62.0 °C
144 °F
ASTM D3418 - ISO 3146
DuPont Elvaloy® HP662 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Melting Point 62.0 °C
144 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Melting Point 62.2 °C
144 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® UL 7710 Adhesive Application Resin
Escorene Ultra UL 7710 is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt ..
Melting Point 62.2 °C
144 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® UL 7710E Adhesive Application Resin
Escorene Ultra UL 7710E is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt..
Melting Point 62.0 °C
144 °F
Freezing Point; ASTM D3418, ISO 3146
DuPont™ Surlyn® E185SB Ionomer Resin
Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed..
Melting Point 62.0 °C
144 °F
DSC, 10°C/min (peak); DuPont Test
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer
Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th..
Melting Point 62.0 °C
144 °F
DSC
Arkema Group EVATANE® 33-45 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-45 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-45 is stabilized with antioxidants. The High Vinyl Acetate co..
Melting Point 62.0 °C
144 °F
DSC
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used..
Melting Point 62.0 °C
144 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Melting Point 62.0 °C
144 °F
ASTM D3418 - ISO 3146
DuPont Elvaloy® HP663 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer  (discontinued **)
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.