Thermal Properties Metric English Comments
Melting Point 149 - 157 °C
300 - 315 °F
Plaskolite Optix® Acrylic Sheet
Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,..
Melting Point 149 - 157 °C
300 - 315 °F
Plaskolite Optix® DA Digital Acrylic Sheet
Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup..
Melting Point 132 - 157 °C
270 - 315 °F
Average value: 150 °C Grade Count:7
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..