Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 871 °C | 1600 °F | |
IBC Advanced Alloys 4% BeCu Beryllium Copper Master Alloy Beryllium copper “Master Alloys†are formulated to introduce relatively small percentage “alloying†additions to base metal furnace melts. Producers of aluminum, magnesium, and n.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; A (TB00) Temper (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Tube; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy M25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM02 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM06 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 871 °C | 1600 °F | |
Heatbath/Park High Speed 60 High Speed Hardening Salt Solution Treating Salt. A neutral salt designed for heat treatment high alloy steels requiring temperatures of 1650° to 2200°F. Formulated per MIL-S-10699-B, Class 6.Information provided by H.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy M25 Wire; H (TD04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | >= 871 °C | >= 1600 °F | approximate |
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit.. |
|||
Melting Point | 870 - 920 °C | 1600 - 1690 °F | |
Wieland 1403 Wilaform Gold Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, lamin.. |
|||
Melting Point | 870 - 930 °C | 1600 - 1710 °F | |
Wieland 1410 Wilaform Gold Yield alloy. Particularly suitable for the production of strongly deformed or thick chains.Applications: casting, chains, coin/shapeDental |
|||
Melting Point | 870 - 890 °C | 1600 - 1630 °F | |
Wieland 1604 Wilaform Gold Rose gold for all kinds of decoration manufacturingApplications: casting, laminar decoration, pipes, tubingDental |