Polymer Property : Melting Point = 930 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 890 - 930 °C
1630 - 1710 °F
Johnson Matthey F Bronze High Temperature Alloy for Tungsten Carbide Brazing
F Bronze is primarily used for the production of rock drills. Or where simultaneous heat treatment of the steel shank is required. Information provided by Johnson Matthey.
Melting Point 800 - 930 °C
1470 - 1710 °F
Wieland 1005 Wilaform Gold
Hard red gold alloy for used in decoration manufacturing.Applications: casting, chains, laminar decorationDental
Melting Point 870 - 930 °C
1600 - 1710 °F
Wieland 1410 Wilaform Gold
Yield alloy. Particularly suitable for the production of strongly deformed or thick chains.Applications: casting, chains, coin/shapeDental