Thermal Properties Metric English Comments
Melting Point 81.0 °C
178 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 3030 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 81.0 °C
178 °F
Exxon Method
ExxonMobil Escorene® LD-722 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr..
Melting Point 81.0 °C
178 °F
Exxon Method
ExxonMobil Escorene® MV 02514 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 14% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Melting Point 81.0 - 83.0 °C
178 - 181 °F
Hong Kun Group UV 328 UV Absorber
UV328 is a strong ultraviolet light absorber in the 290-400nm region. It provides effective light stabilization and prevents the yellowing and degradation of polymers such as PVC, unsaturated polyes..
Melting Point 81.0 - 85.0 °C
178 - 185 °F
Hong Kun Group UV 770 UV Absorber
Chemical Name: bis-(2,2,6,6-Tetramethyl-4-piperidyl) sebacateCAS No. 52829-07-9All information provided by Hongkun Group
Melting Point 81.0 - 85.0 °C
178 - 185 °F
Indium Corp. Indalloy 29 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 81.0 °C
178 °F
Eutectic
Indium Corp. Indalloy 27 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 81.0 - 86.0 °C
178 - 187 °F
Suqian Unitechem Hindered Amine Light Stabilizer 770
Chemical Name: Bis(2,2,6,6-tetramethyl-4-piperidyl)sebaceateCAS NO.: 52829-07-9Molecular Formula: C28H52O4N2Applications: LS770 is recommended to be used in polypropylene, impact modified PP(TPO), E..
Melting Point 81.0 °C
178 °F
TRN-14
Tipco Tipcolite® TPF 1111 - Rubber & Mineral Modified Phenolic Resin, 19 mm Norton Flow with 7% Hexamine
Latex/Mineral Modified Phenolic Resin having 19mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: High Heat BrakeliningInformation provided by the Manufacturer, Tipco Ind..
Melting Point 81.0 °C
178 °F
by DSC; ASTM D3418
Westlake EMAC® SP2202 21.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2202 is a 21.5% EMA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2202 provides exce..
Melting Point 81.0 °C
178 °F
by DSC; ASTM D3418
Westlake EMAC® SP2207 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2207 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficient of friction..
Melting Point 81.0 °C
178 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des..
Melting Point 81.0 °C
178 °F
ASTM D3418, ISO 3146
DuPont™ Elvax® 3178Z Ethylene Vinyl Acetate
DuPont™ Elvax® 3178Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3..
Melting Point 81.0 °C
178 °F
DTA
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
Melting Point 81.0 °C
178 °F
Exxon Method
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate
Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast..
Melting Point 81.0 °C
178 °F
DSC
Arkema Group EVATANE® 18-150 Copolymer Ethylene - Vinyl Acetate
EVATANE® 18-150 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 18-150 is stabilized with antioxidants. The High Vinyl Acetate ..
Melting Point 81.0 °C
178 °F
Exxon Method
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate
Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so..
Melting Point 81.0 °C
178 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3128 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
8.9 wt% Vinyl Acetate.Elvax® 3128 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resin..