Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1927 °C | 3501 °F | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Melting Point | 1927 °C | 3501 °F | |
Zircar Ceramics SALI Moldable Alumina Insulation A close cousin to premium grade Type SALI insulation, SALI Moldable is a thick doughy material readily shaped into complex forms using molds & hand building techniques or applied to surfaces. When .. |
|||
Melting Point | 1927 °C | 3501 °F | |
Unifrax Fiberfrax® 880 Ceramic Fiber Paper 880 paper is made from a higher alumina content, shorter, smaller diameter fiber and laid up at higher densities. These product parameters lead to reduced shrinkage, higher strength, an increased o.. |
|||
Melting Point | 1927 °C | 3501 °F | |
Unifrax Fiberfrax® 882-H Ceramic Fiber Paper This product is completely free of organics and used when higher fired strength is required or in processes and applications where even small amounts of organic burnout is unacceptable. 882-H has h.. |