Polymer Property : Melting Point = 1955 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1029 - 1068 °C
1885 - 1955 °F
Cadi 2 MOLD-MOR™
A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical an..
Melting Point 1029 - 1068 °C
1885 - 1955 °F
Cadi 20 MOLD-MOR™
A Beryllium Copper Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company.
Melting Point 1029 - 1068 °C
1885 - 1955 °F
Cadi C17500 Copper Alloy
Information provided by Cadi Company.