Thermal Properties Metric English Comments
Melting Point 209 °C
408 °F
ASTM D789
NYCOA 1838 Copolymer Nylon Alloy
good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc.
Melting Point 209 °C
408 °F
ISO 3146C
Gromax 1155LL TPE
1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex..
Melting Point 209 °C
408 °F
ASTM D2117
Samyang Triel® 5600 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5600 is an extrusion grade.Information provided by Samyang.
Melting Point 209 - 211 °C
408 - 412 °F
The Chemical Company DICYANDIAMIDE, C2H4N4
Commonly known as DICYandiamide (DICY), the white crystalline compound is the dimer for cyanamide or for cyanoguanidine. The primary use of the chemical is in the production of melamine, but it is a..
Melting Point 209 °C
408 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® HTR8785 BK482 Polyester Elastomer TPC-ET  (Unverified Data**)
Information provided by DuPont Performance Polymers