Thermal Properties Metric English Comments
Melting Point 60.0 - 109 °C
140 - 228 °F
Average value: 87.4 °C Grade Count:12
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..