Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 41C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 43C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 46C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1080 - 1260 °C | 1980 - 2300 °F | |
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness .. |