Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Nucalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness and toughness, similar to the cobalt base alloys . Because of the unique microstructure features, they are less crack sensitive than the conventional nickel-base hardfacing alloys, such as, NiCr-A and NiCr-B, during welding.The Nucalloy alloys have a matrix consisting of, essentially, nickel solid solution, a binary eutectic and ternary eutectic. The binary eutectic is composed of nickel solid solution and nickel silicide (Ni3Si); whereas the ternary eutectic consists of nickel solid solution, nickel boride (Ni3B) and nickel silicide (Ni3Si). There are also carbide and boride particles dispersed in the matrix. The microstructures of these alloys differ from those of the conventional self-fluxing nickel alloys in that the brittle binary eutectic of nickel solid solution and nickel boride does not form because of the intentionally controlled high silicon to boron ratios.The high silicon and low boron in these alloys results in high fractions of nickel silicide, which is resistant to certain corrosive media due to the tendency to form a high-silicon film on the surface.Information provided by Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.10 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 36
36
Hardness, Vickers 410
410
303

@Temperature 700 °C
303

@Temperature 1290 °F
334

@Temperature 600 °C
334

@Temperature 1110 °F
350

@Temperature 500 °C
350

@Temperature 932 °F
363

@Temperature 400 °C
363

@Temperature 752 °F
Tensile Strength, Ultimate 1048 MPa
152000 psi
945 MPa

@Temperature 600 °C
137000 psi

@Temperature 1110 °F
951 MPa

@Temperature 400 °C
138000 psi

@Temperature 752 °F
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 20.0 °C
95.2 ft-lb/in²

@Temperature 68.0 °F
20.0 J/cm²

@Temperature 400 °C
95.2 ft-lb/in²

@Temperature 752 °F
20.0 J/cm²

@Temperature 600 °C
95.2 ft-lb/in²

@Temperature 1110 °F
Thermal Properties Metric English Comments
Melting Point 1080 - 1260 °C
1980 - 2300 °F
Solidus 1080 °C
1980 °F
Liquidus 1260 °C
2300 °F
Component Elements Properties Metric English Comments
Boron, B 0.60 %
0.60 %
Carbon, C 0.30 %
0.30 %
Chromium, Cr 15 %
15 %
Iron, Fe 5.0 %
5.0 %
Nickel, Ni 72 %
72 %
As Remainder
Silicon, Si 5.0 %
5.0 %
Tungsten, W 2.0 %
2.0 %