Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1220 - 1270 °C | 2230 - 2320 °F | |
Special Metals FERRY® Alloy A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy .. |
|||
Melting Point | 1170 - 1270 °C | 2140 - 2320 °F | |
Wieland 1104 Wilaform Gold Silver white gold alloy for all kinds of decoration manufacturing.Applications: casting, chains, coin/shape, laminar decorationDental |