Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, welded and tested as welded Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, weld metal as welded Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Melting Point | 1300 °C | 2370 °F | |
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Melting Point | 1300 °C | 2370 °F | |
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Melting Point | 1300 °C | 2370 °F | |
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Melting Point | 1300 °C | 2370 °F | |
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Melting Point | 1300 - 1370 °C | 2370 - 2500 °F | |
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St.. |
|||
Melting Point | 1300 - 1350 °C | 2370 - 2460 °F | |
Special Metals MONEL® Alloy 400 A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem.. |
|||
Melting Point | 1300 - 1350 °C | 2370 - 2460 °F | |
Special Metals MONEL® Alloy R-405 The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a.. |
|||
Melting Point | 1300 - 1355 °C | 2370 - 2471 °F | |
Special Metals NIMONIC® Alloy 263 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability an.. |
|||
Melting Point | 1300 - 1345 °C | 2370 - 2453 °F | |
Special Metals NIMONIC® Alloy PK33 A nickel-chromium-cobalt alloy that is precipitation hardenable and also contains a relatively high (7%) level of molybdenum for solid-solution strengthening. It has an exceptional combination of h.. |
|||
Melting Point | 1300 °C | 2370 °F | |
Special Metals Nitinol Body-Temperature Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Melting Point | 1300 °C | 2370 °F | |
Special Metals Nitinol Chrome-Doped Superelastic Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Melting Point | 1300 °C | 2370 °F | |
Special Metals Nitinol High-Strength Superelastic Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Melting Point | 1300 °C | 2370 °F | |
Special Metals Nitinol High-Strength Superelastic Ni-Ti-Fe alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Melting Point | 1300 °C | 2370 °F | |
Special Metals Nitinol High-Temperature Shape Memory Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Melting Point | 1300 °C | 2370 °F | |
Special Metals Nitinol High-Temperature Shape Memory Ni-Ti alloy Ribbon Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Melting Point | 1300 °C | 2370 °F | |
Special Metals Nitinol Superelastic Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Melting Point | 1300 - 1350 °C | 2370 - 2460 °F | |
Goodfellow Nickel 70/Copper 30 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Melting Point | 1300 - 1400 °C | 2370 - 2550 °F | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 649°C (1200°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Melting Point | >= 1300 °C | >= 2370 °F | |
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |