Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 125.5 °C | 257.9 °F | Exxon Method |
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Melting Point | 125.5 °C | 257.9 °F | Exxon Method |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Melting Point | 125.5 °C | 257.9 °F | Exxon Method |
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo.. |