ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 430 hour
>= 430 hour
F-50; 10% Igepal Cond. B; ASTM D1693
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.9 MPa
2450 psi
ASTM D638
Elongation at Break 415 %
415 %
ASTM D638
Flexural Modulus 0.579 GPa
84.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 125.5 °C
257.9 °F
Exxon Method
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648