Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 129 °C | 265 °F | ASTM D3418 |
ExxonMobil HD 6510 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3418 |
ExxonMobil HD 6510.17 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total Finathene® 7208 HDPE extrusion resin
(discontinued **) Applications: monofilament, slit tape, woven and knitted fabrics, specialty filmsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics .. |
|||
Melting Point | 129 °C | 265 °F | |
Heatbath/Park Scale Kleen 1259 Descaling Salt A highly alkaline and oxidizing salt bath used specifically as a low temperature bath for descaling titanium and titanium alloys.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total 6410 HDPE Film Resin Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total HDPE BM962 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |