Thermal Properties Metric English Comments
Melting Point 2715 °C
4919 °F
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation
Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par..
Melting Point 2715 °C
4919 °F
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation
Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par..