Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2715 °C | 4919 °F | |
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par.. |
|||
Melting Point | 2715 °C | 4919 °F | |
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par.. |