Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 152 °C | 305 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP PROTEUS® EURO-GRAY Copolymer Polypropylene |
|||
Melting Point | 152 °C | 305 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet) |
|||
Melting Point | 152 °C | 305 °F | |
Heatbath/Park Marquench Quenching and Tempering Salt Low cost quench salt with slightly higher melting point and narrower working range than Low Temp Draw Salt and Thermo-Quench salts. It is as fluid as lower melting salts above 400°F offering equi.. |
|||
Melting Point | 152 °C | 305 °F | |
Heatbath/Park Parcure 305 Rubber Cure Salt Nitrate/Nitrite Salt. A very popular rubber cure salt that combines wide working range with low cost and relatively lower dragout when used above 400°F. (330 Parkettes)Information provided by He.. |