Polymer Property : Melting Point = 315 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 310 - 315 °C
590 - 599 °F
Average value: 311 °C Grade Count:4
Overview of materials for Polyphthalamide (PPA), High Impact
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a..
Melting Point 300 - 315 °C
572 - 599 °F
Average value: 307 °C Grade Count:16
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Melting Point 300 - 315 °C
572 - 599 °F
Zeus PFA Tubing
PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar..
Melting Point 305 - 315 °C
581 - 599 °F
Asahi Glass Fluon® P-66P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melting Point 305 - 315 °C
581 - 599 °F
Asahi Glass Fluon® P-63P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melting Point 305 - 315 °C
581 - 599 °F
Asahi Glass Fluon® P-65P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melting Point 305 - 315 °C
581 - 599 °F
Asahi Glass Fluon® P-802UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melting Point 305 - 315 °C
581 - 599 °F
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melting Point 305 - 315 °C
581 - 599 °F
Asahi Glass Fluon® P-810UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..