Polymer Property : Melting Point = 33.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 33.0 °C
91.4 °F
DSC, 10°C/min; DuPont Test
Dow Engage® 8842 Polyolefin Elastomer
Description: Engage® 8842 polyolefin elastomer is an ultra-low density ethylene-octene copolymer with a nominal loose talc surface coating. The talc is untreated and has a nominal 1 µm particle si..
Melting Point 33.0 - 107 °C
91.4 - 225 °F
Dow Engage® Polyolefin Elastomer
Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. ..