Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 33.0 °C | 91.4 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8842 Polyolefin Elastomer Description: Engage® 8842 polyolefin elastomer is an ultra-low density ethylene-octene copolymer with a nominal loose talc surface coating. The talc is untreated and has a nominal 1 µm particle si.. |
|||
Melting Point | 33.0 - 107 °C | 91.4 - 225 °F | |
Dow Engage® Polyolefin Elastomer Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. .. |