Thermal Properties Metric English Comments
Melting Point 360 - 382 °C
680 - 720 °F
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Melting Point 360 °C
680 °F
DSC
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Melting Point 360 °C
680 °F
DSC
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade
Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II.
Melting Point 360 °C
680 °F
DSC
Performance Polymers IPS II PPL-C4250 PEKK (Polyetherketoneketone) Linear 30% Carbon Fiber Reinforced Molding Grade
Black pelletsInformation provided by Infinite Polymer System II.
Melting Point 360 °C
680 °F
DSC
Performance Polymers IPS II PPL-C4270 PEKK (Polyetherketoneketone) Linear 40% Carbon Fiber Reinforced Molding Grade
Black pelletsInformation provided by Infinite Polymer System II.
Melting Point 360 °C
680 °F
DSC
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Melting Point 360 °C
680 °F
DSC
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Melting Point 360 - 1030 °C
680 - 1890 °F
Indium Corp. Indalloy 199 Gold Solder Alloy
Information Provided by Indium Corporation