Thermal Properties Metric English Comments
Melting Point 207 °C
405 °F
ISO 3146C
Gromax 1140LH TPE
Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject..
Melting Point 207 °C
405 °F
ASTM D2117
Samyang Triel® 5552EM Thermoplastics Polyetherester Elastomer, Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5552EM is an extrusion grade.Information provided by Samyang.
Melting Point 207 °C
405 °F
DSC
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Melting Point 207 °C
405 °F
Crystalline Peak; ASTM D3418
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Melting Point 207 °C
405 °F
Crystalline Peak Melting Point; ASTM D3418
Eastman Neostar FN005 Elastomer
Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough..
Melting Point 207 °C
405 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 207 °C
405 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point <= 207 °C
<= 405 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b..
Melting Point 207 °C
405 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 207 °C
405 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 207 °C
405 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
Melting Point 207 °C
405 °F
ASTM D789
Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced
A glass fiber reinforced, flame retardant PBT exhibiting excellent strength, dimensional stability and elevated temperature performance. The material has a V0 flammability rating according to UL94 ..