Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 184 - 210 °C | 363 - 410 °F | |
Indium Corp. Indalloy® 7 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Melting Point | 177 - 210 °C | 351 - 410 °F | |
Indium Corp. Indalloy 115 Tin-Lead Solder Alloy Information Provided by Indium Corporation |