Polymer Property : Melting Point = 4170 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 2300 °C
4170 °F
Specialty Materials Boron Monofilament
Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information prov..
Melting Point 2300 - 2400 °C
4170 - 4350 °F
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..