Polymer Property : Melting Point = 420 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 420 - 480 °C
788 - 896 °F
Solvay Chemicals (CsAlF4) Cesium Tetrafluoroaluminate
Flux for brazing aluminum. Particularly suitable for flame brazing of magnesium-containing aluminum alloys.HS No.: 38109090 /CAS-No.: 39211-00-2Uses: Automotive Sector, Commercial & Residential Ai..
Melting Point 420 °C
788 °F
via DSC
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo..
Melting Point 420 - 480 °C
788 - 896 °F
Solvay Chemicals (CsAlF-Complex) Cesium Fluoroaluminate
Low-melting-point flux for brazing aluminum.HS No.: 38109090 /CAS-No.: 138577-01-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl..