Thermal Properties Metric English Comments
Melting Point 237 - 247 °C
459 - 477 °F
Indium Corp. Indalloy® 236 Pb-Sb-Sn-Ag Solder Alloy
Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation.
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 20-05HH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade)
Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melting Point <= 237 °C
<= 459 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin
Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p..
Melting Point 237 °C
459 °F
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE
Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.