Material Notes:
Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 2.11 g/cc
0.0762 lb/in³
ISO 1183
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ISO 868
Ball Indentation Hardness 48.0 MPa
6960 psi
ISO 2039-1
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Elongation at Break 120 %
120 %
ISO 527
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Specific Heat Capacity 1.00 J/g-°C
0.239 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Melting Point 237 °C
459 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 370 °C
698 °F
Molding
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure