Polymer Property : Melting Point = 500 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point >= 500 °C
>= 932 °F
via DSC
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating
Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4..
Melting Point 500 °C
932 °F
Goodfellow Zinc 95/Copper 5 Alloy
Information provided by Goodfellow.